Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman Aqua 20837 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20.. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman 15041 PET
(discontinued **) Voridian polymer 15041 is a PET thermoplastic polyester.Applications/UsesCrystallized PET (CPET) trays |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman 9663 PET
(discontinued **) VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers.. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman BD445 PET
(discontinued **) Voridian Polymer BD445 is primarily targeted for the soft drink and water markets, it is also suitable for use in other beverage containers as well as food and on-food-related applications. This pol.. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman CA12 PET
(discontinued **) Voridian Polymer CA12 is currently produced to Voridian’s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer CA12 offers imp.. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman CB12 PET
(discontinued **) Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov.. |
|||
Specific Heat Capacity | 1.90 J/g-°C | 0.454 BTU/lb-°F | |
Americas Styrenics Styron® 6010 High Impact Polystyrene
(discontinued **) STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac.. |
|||
Specific Heat Capacity | 1.90 J/g-°C | 0.454 BTU/lb-°F | |
Micropol Isoplas P381 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Specific Heat Capacity | 1.90 J/g-°C | 0.454 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Polidan® S/I 20 Polyethylene, Crosslinked (XLPE) POLIDAN® S/I 20 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for injection molding.Features: Crossl.. |
|||
Specific Heat Capacity | 1.90 J/g-°C | 0.454 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE) POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features.. |
|||
Specific Heat Capacity | 1.90 J/g-°C | 0.454 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Specific Heat Capacity | 1.90 J/g-°C | 0.454 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Specific Heat Capacity | 1.90 J/g-°C | 0.454 BTU/lb-°F | |
Styron Magnum™ 4455 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
DSC |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Specific Heat Capacity | 1.90 J/g-°C | 0.454 BTU/lb-°F | of Liquid |
BASF Isobutyl Acrylate Formula: C7H12O2CAS: 106-63-8Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Isobutyl acrylate forms homopolymers and copolymers. Copol.. |
|||
Specific Heat Capacity | 1.90 J/g-°C | 0.454 BTU/lb-°F | DSC |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Specific Heat Capacity | 1.90 J/g-°C | 0.454 BTU/lb-°F | |
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Specific Heat Capacity | 1.90 - 2.30 J/g-°C @Temperature 100 - 175 °C |
0.454 - 0.550 BTU/lb-°F @Temperature 212 - 347 °F |
Average value: 2.10 J/g-°C Grade Count:1 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman 5214A PET
(discontinued **) Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe.. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Specific Heat Capacity | 1.90 J/g-°C @Temperature 200 °C |
0.454 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Specific Heat Capacity | 1.90 - 2.30 J/g-°C @Temperature 100 - 175 °C |
0.454 - 0.550 BTU/lb-°F @Temperature 212 - 347 °F |
Average value: 2.10 J/g-°C Grade Count:3 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |