Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.88 J/g-°C | 0.449 BTU/lb-°F | Melt |
Covestro Makroblend® S 7916 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PBT+PC)-blendsimpact modifiedInjection molding gradeexcellent chemical resistancehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessing.. |