Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.406 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Apec® 2000 Polycarbonate  (discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Apec® DP 1-9379/5 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Apec® DP 1-9389 Polycarbonate  (discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and ha..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
DIN 52612
Zell-Metall Engineering Plastics Zellamid 202 (PA 6)
Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased...
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Apec® 1745 Polycarbonate
Easy to demoldsuitable for superheated steam sterilization up to 143 °C as well as for pharmaceutical applications according to United States Pharmacopeia (USP) XXII Class VIsoftening temperature (..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Apec® 1795 Polycarbonate
Easy flowingeasy to demoldsoftening temperature (VST/B 120)=173°CPreprocessingMax. Water content
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Apec® DP1-9389/5 Polycarbonate
Developmental producteasy flowingeasy to demoldsoftening temperature (VST/B 120)=218 °CPreprocessingMax. Water content
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Bayblend® KU 2-1514 BBS073* Polycarbonate + ABS, Flame Retardant Grade
Developmental productHigh heat resistant injection molding gradeimproved chemical resistance and stress cracking behavior compared to KU 2-1514ball indentation temperature = 125 °CVicat/B 120 tempe..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Desmopan® DP 1080A Polyurethane
injection molding gradefree from plasticizershard - soft systemsTechnical partsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covest..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Desmopan® DP 2786A Polyurethane
Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Desmopan® DP 2792A Polyurethane
Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Desmopan® DP 8798A Polyurethane
injection molding gradewith special UV stabilizersEasy releaseshort cycle timesApplicationSports shoe solesPreprocessingMax. Water content
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Desmopan® DP 9370A Polyurethane
Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilityfree from plasticizershigh moisture vapor transmission rateApplicationbreathable fi..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Desmopan® DP 9380A Polyurethane
Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilitycomplies with VDE 0282-10ApplicationCable sheathingsHosesnon-reinforcedPreprocessin..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Desmopan® W DP 85085A Polyurethane
injection molding gradeno yellowing under the action of UV lightimproved microbial resistancegood low-temperature flexibilityImproved hydrolysis resistanceApplicationautomotive interior applications..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® 1899* Polycarbonate, Impact Grade
Formerly Makrolon DP1-1899MVR (300 °C/1.2 kg) 15.5 cm³/10 minspecial flame retardant systemUL 94V-0/0.75 mmImpact modifiedMedium viscosityEasy releaseVicat softening temperature 50 N; 50 °C/h = 1..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® 2856 Polycarbonate
ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAva..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® 2865 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt tempe..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® 2867 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt tem..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® 3107 Polycarbonate
ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minGeneral purposeHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpare..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® 3156 Polycarbonate
ISO 7391-PC,MR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtru..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® AG2677 Polycarbonate
ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transparent colors on..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® LED2045 Polycarbonate
ISO 7391-PC,MRT,(,,)-24-9Global gradeMVR (250 °C/2.16 kg) 16.5 cm3/10minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable ..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® Rx1805 Polycarbonate
ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® Rx2430 Polycarbonate
ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 an..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Hippe PP Polypropylene
Lower density compared with PE. Higher hardness and stiffness and better reset features. Non-fragile. Toughness in cold lesser than that of PE. Higher working temperatures than PE, not aromatic-..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® DP1-1825* Polycarbonate, Impact Grade
Developmental productISO 7391-PC,MP,(,,)-09-9MVR (300 °C/1.2 kg) 6.0 cm3/10 minImpact modifiedHigh viscosityInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPreproce..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® LQ3187 Polycarbonate
ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable i..
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
BASF Ultramid® C3U PA66/6 (Dry)
Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance.
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Covestro Makrolon® LQ2687 Polycarbonate
ISO 7391-PC,MLR,(,,)-18-9MVR (300 °C/1.2 kg) 12.5 cm3/10 minOptical lensMedium viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear t..
Copyright © lookpolymers.com All Rights Reserved