Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
ASTM E1269 |
Eastman CB11E PET
(discontinued **) VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and bet.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer
(discontinued **) Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | DSC |
Eastman Eastobond 19411 Copolyester, Film Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low so.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | DSC |
Eastman Neostar FN005 Elastomer Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | DSC |
Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | Melt |
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | Melt |
Covestro Makrolon® GF9002* Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-18-9,GF10Formerly Makrolon DP1-1889MVR (300 °C/1.2 kg) 15 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.2 mmUL 94 5VA/2.8 mm (Bayer .. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | Melt |
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | IEC 1006 |
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | IEC 1006 |
BASF Ultradur B 4300 G4 20% Glass Filled PBT Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | IEC 1006 |
BASF Ultradur® B 4406 G2 10% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 10% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |
|||
Specific Heat Capacity | 1.60 J/g-°C @Temperature 100 °C |
0.382 BTU/lb-°F @Temperature 212 °F |
|
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Specific Heat Capacity | 1.60 J/g-°C | 0.382 BTU/lb-°F | IEC 1006 |
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |