Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Plaskolite PL-24 Acrylic Resin For injection molding. An unlubricated version of PL-25 extrusion grade pellets. Highest molecular weight, maximum heat resistance.Information supplied by the manufacturer. |
|||
Specific Heat Capacity | 1.46 - 1.50 J/g-°C | 0.349 - 0.359 BTU/lb-°F | Average value: 1.47 J/g-°C Grade Count:9 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Diapolyacrylate Acrypet® MF-001 PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Diapolyacrylate Acrypet® VH-001 Heat Stabilized PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Diapolyacrylate Acrypet® IR H70 Impact Modified PMMA Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Asahi Kasei Delpet® 560F Acrylic Molding Compound 560F has the highest flow of Delpet® grades, allowing reduced screw load for broad selection of molding conditions. General Delpet® qualities include attractive transparency, elegant luster and c.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Asahi Kasei Delpet® 60N Acrylic Molding Compound 60N is a medium grade of heat resistance and mechanical strength, allowing injection molding through relatively small gates and runners. General Delpet® qualities include attractive transparency, .. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Asahi Kasei Delpet® 80N Acrylic Molding Compound, High Heat Grade 80N has high heat resistance and strength. Recommended for taillight lenses, reflectors, and other auto parts, and general lighting fixtures. General Delpet® qualities include attractive transpar.. |
|||
Specific Heat Capacity | 1.46 J/g-°C | 0.349 BTU/lb-°F | |
Lucite International SW Sanitary Ware Acrylic Sheet Lucite® SW complies with ISO 7823-1 and EN 263. It is approved by the French ARNOR "NF" quality mark.Information provided by Lucite International |