Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203 PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 223R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 4701R PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. |
|||
Specific Heat Capacity | 1.26 J/g-°C @Temperature 4.00 °C |
0.301 BTU/lb-°F @Temperature 39.2 °F |
ASTM E1269 |
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Specific Heat Capacity | 1.26 J/g-°C @Temperature 4.00 °C |
0.301 BTU/lb-°F @Temperature 39.2 °F |
ASTM E1269 |
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2114 PC (Asia Pacific) 18 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East) Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2414G PC (Asia Pacific) 10 MFR. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Specific Heat Capacity | 1.26 - 1.70 J/g-°C @Temperature 50.0 - 200 °C |
0.301 - 0.406 BTU/lb-°F @Temperature 122 - 392 °F |
Average value: 1.47 J/g-°C Grade Count:5 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 243 PC 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 243 PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.301 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 243R PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 285E3720005 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 307E0V16310 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Specific Heat Capacity | 1.26 - 1.67 J/g-°C | 0.301 - 0.399 BTU/lb-°F | DSC |
Eastman Tenite 360A4861301 Propionate Clear, Trsp
(discontinued **) Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |