Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 20 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 30 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 400 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 600 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9040 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9070 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9235 High Performance Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9275 High Performance Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® R10450 Medium Fiberglass Reinforced Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® R10460 Medium Flame Retardant Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® R10470 Firm General-Purpose Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® R10470 Medium General-Purpose Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® R10480 Medium Low Compression Set Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® R10480 Soft Low Compression Set Silicone Sponge Rubber Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six cons.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® R10490 Medium Fluorosilicone Sponge Rubber Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six constructions. R1.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 300 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 500 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 700 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9030 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9050 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9060 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Saint-Gobain COHRlastic® 9255 High Performance Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Ensinger Tecanat™ Unfilled Polycarbonate (PC) Tenacat™ is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for pumps.. |
|||
Specific Heat Capacity | 1.26 J/g-°C | 0.300 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |