Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 101R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 104 PC (Asia Pacific) LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 104R PC (Asia Pacific) LEXAN 104R is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information a.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 121 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 121R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® 134 PC Nonhalogenated. 3.5 MFR. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® 135 PC General purpose low flow polycarbonate powder gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 153 PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® 221 PC 17.5 MFR, for small, intricate parts. Improved flame retardance.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 221R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® 223 PC 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 244R PC (Asia Pacific) LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPS2S PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® PK2870 PC (Asia Pacific) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® VR2020 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 143 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 143 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 144R PC (Asia Pacific) LEXAN 144R is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® 151 PC Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 4501 PPC High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® FXE143R PC UV stabilized PC resin for "Illuminate"/Edge Glow Visual Effect. Medium viscosity (10.5 MFR). Nonhalogenated.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | ASTM C 351 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Heat Capacity | 1.25 J/g-°C | 0.299 BTU/lb-°F | |
IBC Advanced Alloys Beralcast® 363 Beryllium-Aluminum Alloy This alloy provides an ideal solution for weight, stiffness and thermal critical applications in aerospace, defense and commercial markets. BeAl-363 is a metal matrix composite which consists of 65%.. |