Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 500 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 500 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 500R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 500R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 503 PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 503R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 503R PC (Asia Pacific) 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
Specific Heat Capacity | 1.21 - 1.81 J/g-°C | 0.289 - 0.433 BTU/lb-°F | Average value: 1.40 J/g-°C Grade Count:6 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | R&H P-37 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Hippe PBT Polybutylene Terephthalate The mechanical properties of PBT are generally inferior to the partially crystallized PET, however, PBT is more easily machined.Information provided by Hippe. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Azoty Tarnow™ TARNOFORM 300 GF4 POM 20% glass fiber reinforced injection molding grade with very high strength.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Azoty Tarnow™ TARNOFORM 300 GF6 POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Azoty Tarnow™ TARNOFORM 300 GF7 POM 35% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
Azoty Tarnow™ TARNOFORM 500 GF6 POM 30% glass fiber reinforced, high flow injection molding grade, suitable for applications where high strength and stiffness is required, combined with higher flowability during molding.Information pr.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
3M Novec™ 7200 Engineered Fluid 3M™ Novec™ 7200 fluid's convenient boiling point and excellent environmental, health and safety profile make it useful as a heat transfer fluid, cleaning solvent, for lubricant deposition & many m.. |
|||
Specific Heat Capacity | 1.21 J/g-°C | 0.289 BTU/lb-°F | |
3M Novec™ 7200DL Engineered Fluid A high-purity version of 3M™ Novec™ 7200, 3M™ Novec™ 7200DL is tightly-controlled for ions, metals and non-volatile residue. It is used when an application calls for high-purity materials, or a .. |