Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Osprey Metals CE11 Al-Si Controlled Expansion Alloy Al-50%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
Specific Heat Capacity | 0.795 J/g-°C | 0.190 BTU/lb-°F | |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Specific Heat Capacity | 0.796 J/g-°C | 0.190 BTU/lb-°F | |
MMCC Aluminum/SiC 55p Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT110 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT120 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Specific Heat Capacity | 0.795 J/g-°C @Temperature 20.0 - 800 °C |
0.190 BTU/lb-°F @Temperature 68.0 - 1470 °F |
|
Zircar Ceramics MICROSIL Microporous Insulation MICROSIL Microporous Insulation is an insulation material. Having thermal conductivity an order of magnitude lower than ceramic fiber materials Microsil Microporous Insulation can be an integral par.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT140 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT160 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT180 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT350 Boron Nitride (BN) Powder Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT370 Boron Nitride (BN) Powder Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT620 Boron Nitride (BN) Powder High Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Specific Heat Capacity | 0.794 J/g-°C | 0.190 BTU/lb-°F | |
Momentive Performance Materials PolarTherm® PT670 Boron Nitride (BN) Powder High Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |