Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | |
GrafTech eGRAF® SPREADERSHIELD™ SS1500 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | |
GrafTech eGRAF® SPREADERSHIELD™ SS300 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | |
GrafTech eGRAF® SPREADERSHIELD™ SS400 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | |
GrafTech eGRAF® SPREADERSHIELD™ SS500 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | |
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate.. |
|||
Specific Heat Capacity | 0.700 J/g-°C @Temperature 0.000 - 50.0 °C |
0.167 BTU/lb-°F @Temperature 32.0 - 122 °F |
|
Momentive Performance Materials Type 219 Fused Quartz Tubing Known as "Ozone-Free" or "Germicidal" quartz tubing. Transmits UV-A and UV-B while blocking the deep, high energy wavelengths that cause ozone generation and pose the greatest exposure risks. Tran.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | |
Skamol Group ISOPERLOR 550P Perlite Insulating Brick & Block ISOPERLOR perlite insulating bricks & blocks have the following characteristics: Max. service temperature 900°C (1652°F)Back-up insulation onlyExcellent insulating propertiesVery lightweight a.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | |
Skamol Group Moler HIPOROS Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Specific Heat Capacity | 0.700 J/g-°C @Temperature 100 - 200 °C |
0.167 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 701 Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | DINV ENV 821-3 |
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2 DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | DINV ENV 821-3 |
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3 SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads an.. |
|||
Specific Heat Capacity | 0.700 J/g-°C @Temperature 100 - 200 °C |
0.167 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3 SL 200 ST is a silicon nitride ceramic especially suitable for components exposed to mechanical stress and engine-specific applications even at elevated temperatures. It is recognized for its high s.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | DINV ENV 821-3 |
CeramTec SL 303 Silicon Nitride, SiAION+SiC SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i.. |
|||
Specific Heat Capacity | 0.700 J/g-°C @Temperature 100 - 200 °C |
0.167 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 192/193 Titania 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | ASTM E1269 |
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2) Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | silicone property; ASTM E 1461-1 |
Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | silicone property; ASTM E 1461-1 |
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | E 1461-01 |
Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primerRecommended Primers: Dow Corning S2260Design/Construction: Liner: FEP Product: Uncured S.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | E 1461-01 |
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val.. |
|||
Specific Heat Capacity | 0.700 J/g-°C @Temperature 100 - 200 °C |
0.167 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 447 Cordierite, 2MgO•Al2O3•5SiO2 Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | |
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2) Te value is 670°C. Hasselman Thermal Shock value is 800 K.Data provided by CeramTec North America. |
|||
Specific Heat Capacity | 0.700 J/g-°C | 0.167 BTU/lb-°F | |
CeramTec 965 Toughened Alumina (Al2O3-ZrO2) Hasselman Thermal Shock value is 270 K.Data provided by CeramTec North America. |