Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.667 J/g-°C @Temperature 1100 °C |
0.159 BTU/lb-°F @Temperature 2010 °F |
|
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.667 J/g-°C @Temperature 1100 °C |
0.159 BTU/lb-°F @Temperature 2010 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.667 J/g-°C @Temperature 1100 °C |
0.159 BTU/lb-°F @Temperature 2010 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.667 J/g-°C @Temperature 1100 °C |
0.159 BTU/lb-°F @Temperature 2010 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.667 J/g-°C @Temperature 1100 °C |
0.159 BTU/lb-°F @Temperature 2010 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.667 J/g-°C @Temperature 1100 °C |
0.159 BTU/lb-°F @Temperature 2010 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.665 J/g-°C | 0.159 BTU/lb-°F | ASTM E1269 |
CoorsTek Pure SiC™ HR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |
|||
Specific Heat Capacity | 0.665 J/g-°C | 0.159 BTU/lb-°F | ASTM E1269 |
CoorsTek Pure SiC™ LR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |