Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.5397 J/g-°C @Temperature 0.000 - 100 °C |
0.1290 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Indium Corp. In2(SO4)3 Indium Sulfate Anhydrous Indium Sulfate is a grayish-white powder. It is hydroscopic and possesses a monoclinic prism structure. It is available as an anhydrous powder, a hydrated salt with 9 moles of associated water, an.. |