Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.540 J/g-°C @Temperature 700 °C |
0.129 BTU/lb-°F @Temperature 1290 °F |
|
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Specific Heat Capacity | 0.540 J/g-°C @Temperature 700 °C |
0.129 BTU/lb-°F @Temperature 1290 °F |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Specific Heat Capacity | 0.540 J/g-°C @Temperature 700 °C |
0.129 BTU/lb-°F @Temperature 1290 °F |
|
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 400 °C |
0.129 BTU/lb-°F @Temperature 752 °F |
|
Haynes 214® alloy, 0% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 400 °C |
0.129 BTU/lb-°F @Temperature 752 °F |
|
Haynes 214® alloy, 10% cold reduction Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 400 °C |
0.129 BTU/lb-°F @Temperature 752 °F |
|
Haynes 214® alloy, 10% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 400 °C |
0.129 BTU/lb-°F @Temperature 752 °F |
|
Haynes 214® alloy, 20% cold reduction, 1095°C (2000°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 400 °C |
0.129 BTU/lb-°F @Temperature 752 °F |
|
Haynes 214® alloy, 50% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 400 °C |
0.129 BTU/lb-°F @Temperature 752 °F |
|
Haynes 214® alloy, sheet, 100 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 400 °C |
0.129 BTU/lb-°F @Temperature 752 °F |
|
Haynes 214® alloy, sheet, 1000 hours exposure at 760°C (1400°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 400 °C |
0.129 BTU/lb-°F @Temperature 752 °F |
|
Haynes 214® alloy, sheet, 32 hours exposure at 870°C (1600°F) Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.540 J/g-°C @Temperature 700 °C |
0.129 BTU/lb-°F @Temperature 1290 °F |
|
Haynes 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 400 °C |
0.129 BTU/lb-°F @Temperature 752 °F |
|
Haynes 214® alloy, 30% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, 0% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, 10% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, 10% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, 10% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, 30% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, 30% cold reduction, 1065°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, 40% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, all-weld metal GTAW Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, bar, after 1000 hours at 650°C (1200°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, bar, after 4000 hours at 650°C (1200°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, bar, after 4000 hours at 760°C (1400°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, bar, after 8000 hours at 760°C (1400°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, 20% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, 30% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, 50% cold reduction, 1065°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, bar after 16000 hours at 871°C (1600°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Specific Heat Capacity | 0.538 J/g-°C @Temperature 500 °C |
0.129 BTU/lb-°F @Temperature 932 °F |
|
Haynes 556® alloy, sheet after 1000 hours at 871°C (1600°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |