Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.490 J/g-°C | 0.117 BTU/lb-°F | |
Schott N-LASF41 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.490 J/g-°C | 0.117 BTU/lb-°F | |
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 538°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
Specific Heat Capacity | 0.490 J/g-°C | 0.117 BTU/lb-°F | |
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 593°C High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
Specific Heat Capacity | 0.490 J/g-°C | 0.117 BTU/lb-°F | |
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
Specific Heat Capacity | 0.490 J/g-°C | 0.117 BTU/lb-°F | |
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Overaged High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer.. |
|||
Specific Heat Capacity | 0.490 J/g-°C @Temperature 100 °C |
0.117 BTU/lb-°F @Temperature 212 °F |
|
ATI Allegheny Ludlum AL 304DA Stainless/Carbon Steel Three-Ply Composite Composition above represents only the Type 304 cladding. Its iron content calculated as balance.Allegheny Ludlum AL 304DA is tri-ply composite consisting of a dual stabilized, low carbon steel cent.. |