Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Latrobe Lescalloy® 410Cb High Strength Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
Specific Heat Capacity | 0.462 J/g-°C | 0.110 BTU/lb-°F | RT |
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Specific Heat Capacity | 0.461 J/g-°C | 0.110 BTU/lb-°F | |
Special Metals BRIGHTRAY® Alloy B Electrical Resistance Alloy A nickel-iron-chromium electrical-resistance alloy for use at operating temperatures up to 2010°F (1100°C). It contains rare-earth additions for increased oxidation resistance, especially und.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, .. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 440B Chromium Steel Crucible 440B Is a hardenable chromium steel which is cutlery grade having high attainable hardness and toughness. This grade is magnetic at all times. Information provided by Crucible Specialty Me.. |
|||
Specific Heat Capacity | 0.460 - 0.602 J/g-°C @Temperature 22.2 - 699 °C |
0.110 - 0.144 BTU/lb-°F @Temperature 72.0 - 1290 °F |
|
Dura-Bar 120-90-02 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
Bohler-Uddeholm BÖHLER S400(M7) High Speed Steel Description: High alloyed molybdenum high speed steel with good resistance and high toughness.Applications: Taps, twist drills, reamers, milling tools, broaches tools, cold extrusion dies.Standards:.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
hardened to 310 HB |
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel Cr-Mo alloyed steelP20 Modified offers the following benefits:No hardening risksNo hardening costsTime saving, e.g. no waiting for heat treatmentLower tool cost (e.g. no distortion to rectify)Modifi.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
hardened to 52 HRC |
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel Polmax is an excellent choice for extreme surface finish requirements. This high performance grade achieves surface finishes that go well beyond conventional tool steels. Polmax is specifically eng.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
hardened to 62 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 10 SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel Chromium-molybdenum-vanadium alloyed steelUddeholm Vanadis 10 is a high vanadium alloyed powder metallurgy tool steel offering a unique combination of an excellent abrasive wear resistance in combin.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
hardened to 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
California Fine Wire Nickel 220 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
California Fine Wire Nickel 5900 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
California Fine Wire Stablohm 610 Nickel, Chromium and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
AK Steel 400 Ferritic Stainless steel AK Steel 400 is one of the most economical chromium ferritic stainless steels. It has corrosion and oxidation resistance comparable to Type 410 stainless steel with good fabricating characteristics.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
AK Steel 420 Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
AK Steel 420HC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Assab Steels ASSAB XW-41 Cold Work Steel XW-41 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength Good through-hardening propertiesHigh stability i.. |
|||
Specific Heat Capacity | 0.460 J/g-°C | 0.110 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LXN™ (UNS S31726) Allegheny Ludlum's 317LXN™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Assab Steels 618 Plastic Mold Material ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu.. |