Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C (1350°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C/8hr/FC to 621°C/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/4hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Cold Drawn 37.5% Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Cold Drawn 37.5% Plus Aging 649°C (1200°F)/4hr/FC to 579°C/4hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 718°C (1325°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 746°C (1375°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |