Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.393 J/g-°C @Temperature 20.0 °C |
0.0939 BTU/lb-°F @Temperature 68.0 °F |
|
California Fine Wire Nico Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |