Thermal Properties Metric English Comments
Specific Heat Capacity 0.389 J/g-°C
0.0930 BTU/lb-°F
Kennametal Stellite Stellite® 33
Completely non-magnetic. Specific Electrical Resistance: 39.8 µOhm/in^3.Applications: standard tool bits, tipped tools, form tools, milling cutter blades, wood working tools, reamer blades, cut-o..
Specific Heat Capacity 0.389 J/g-°C
0.0930 BTU/lb-°F
Schott SF6 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.389 J/g-°C
0.0930 BTU/lb-°F
Schott SF6HT Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.389 J/g-°C
0.0930 BTU/lb-°F
Weartech International WT-190 Cobalt Hardfacing & Wear Resistant Alloy
Applications: tri-cone rock bits for oil drillingInformation provided by Weartech International
Specific Heat Capacity 0.389 J/g-°C
0.0930 BTU/lb-°F
Weartech International WT-20 Cobalt Hardfacing & Wear Resistant Alloy
Applications: marine engine valves, control valves for petrochemicals, steel mill rolls, homogenizer valve componentsInformation provided by Weartech International
Specific Heat Capacity 0.389 J/g-°C

@Temperature 100 °C
0.0930 BTU/lb-°F

@Temperature 212 °F
Schmolz + Bickenbach MoldMAX XL® Copper Alloy
Description: Brush Wellman’s MoldMAX XL® is a high strength copper mold alloy with good thermal conductivity. The alloy contains no beryllium and is available in sections as large as 12” thick. ..