Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.381 J/g-°C | 0.0910 BTU/lb-°F | |
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |