Polymer Property : Specific Heat Capacity = 0.0526 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.220 J/g-°C
0.0526 BTU/lb-°F
Nihon Superior SN100C Lead-Free Solder Alloy
Allows high productivity in soldering processes and cost effective, reliable joints. Attributes include high fluidity, low copper erosion, low drossing, superior wetting and freedom from shrinkage d..
Specific Heat Capacity 0.220 J/g-°C
0.0526 BTU/lb-°F
Nihon Superior SN100CL Lead-Free Solder Alloy
Used for hot air solder leveling (HASL). Features include: Excellent fluidity; Bridge-free coating of the fine pitch circuitry; Bright smooth and uniform coating; Low copper erosion; Formation of st..