Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.50 - 1.85 J/g-°C | 0.359 - 0.442 BTU/lb-°F | Average value: 1.65 J/g-°C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |