Thermal Properties Metric English Comments
Specific Heat Capacity 1.00 - 1.20 J/g-°C
0.239 - 0.287 BTU/lb-°F
Average value: 1.13 J/g-°C Grade Count:3
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..