Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 3.89 J/g-°C | 0.930 BTU/lb-°F | Melt value |
BASF Capron® 1943 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 1943 is a type 6 nylon graft copolymer developed for injection molding applications requiring improved dry as molded toughness, and increased flexibility. It has an excellent thermal and che.. |
|||
Specific Heat Capacity | 3.89 J/g-°C | 0.930 BTU/lb-°F | Melt value |
BASF Capron® BG50XFI Impact Modified Nylon 6 (Dry)
(discontinued **) Capron BG50XFI is an injection molding type 6 nylon graft copolymer with superior impact resistance and flow especially for thinner walled parts and long flow lengths. It is also available in natura.. |