Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.89 J/g-°C | 0.452 BTU/lb-°F | |
Styron Magnum™ 357HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Specific Heat Capacity | 1.89 J/g-°C | 0.452 BTU/lb-°F | of Liquid |
BASF 2- Ethylhexyl Acrylate Formula: C11H20O2CAS: 203-080-7Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: 2-Ethylhexyl acrylate forms homopolymers and copolymers. .. |
|||
Specific Heat Capacity | 1.89 J/g-°C | 0.452 BTU/lb-°F | Melt value |
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |