Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.339 J/g-°C @Temperature 300 °C |
0.3200 BTU/lb-°F @Temperature 572 °F |
DSC |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |