Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman A12 PET
(discontinued **) Voridian Polymer A12 is currently produced to Eastman`s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer A12 is available i.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | IES 1006 |
Polycasa LENTICULAR PETG Good ink adhesionGood receptabilityStable sheet dimensionsHigh impact strengthGood chemical resistanceEnvironmentally safeRecyclableMeets current food contact legislationDisplays Graphic Arts Advert.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM D2766 |
Polycasa PETG QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits o.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 0900 Unsaturated Polyester UP BMC 0900 is a special BMC used in a chemically aggressive environment. The glass content is set to a level that combines good mould ability with good strength and stiffness properties. Typical appli.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 1100 Unsaturated Polyester UP BMC 1100 is a special BMC for high strength application. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. The selection of the r.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 2310 Unsaturated Polyester UP BMC 2310 is a chemically resistant grade reinforced with special fibres. Being completely glass-free (no glass fibre reinforcement) it is specifically recommended for the manufacture of high voltage.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® HPC 1200 Unsaturated Polyester UP HPC 1200 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0421 Unsaturated Polyester UP SMC 0421 is a low density premium Class-A SMC for on-line painted exterior body applications on cars. These compounds mould to light weight parts with excellent surface quality for on-line painted .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Haveg 41NA Phenolic; Silicate Filled A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers. |
|||
Specific Heat Capacity | 1.10 J/g-°C @Temperature 100 - 200 °C |
0.263 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 665 Steatite, MgO•SiO2 Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. 665 L533C has low dielectric loss. It makes exc.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | Liquid |
3M Fluorinert™ FC-3283 Electronic Liquid 3M™ Fluorinert™ Liquid FC-3283 is a non-conductive, thermally and chemically stable liquid ideal for use in single phase heat transfer applications, especially in the electronics and semiconductor.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | Liquid |
3M Fluorinert™ FC-70 Electronic Liquid Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
CeramTec 645 Steatite (MgO-SiO2) Te value is 810°C. Hasselman Thermal Shock value is 600 K.Data provided by CeramTec North America. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman VersaTray 12822 Plastic
(discontinued **) VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman 9921W PET Injection Molded