Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | Calculated |
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits: |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA 120 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Sapco C 410 Steatite Information provided by Sapco. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C | 0.215 - 0.263 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Sapco C 221 Steatite Information provided by Sapco. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
CeramTec 771 94% Alumina (Al2O3) Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | DINV ENV 821-3 |
CeramTec B 601 Alumina, 98.5% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 100 - 200 °C |
0.215 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 20.0 - 100 °C |
0.215 BTU/lb-°F @Temperature 68.0 - 212 °F |
DINV ENV 821-3 |
CeramTec Rubalit® IS 95 Alumina Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva.. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | DINV ENV 821-3 |
CeramTec V 679 Alumina, 99.7% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | DSC |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 100 °C |
0.215 BTU/lb-°F @Temperature 212 °F |
Silicone Property; ASTM E 1952 |
Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Arkema Group VOLTALEF® 302 PCTFE VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group |
|||
Specific Heat Capacity | 0.900 J/g-°C | 0.215 BTU/lb-°F | |
Aleris 55HX® Aluminum (5005-H14) Used in interior and exterior architectural applications such as façades and claddings, ceilings and walls, and roofs. Attributes include: anodizing free of streaks; color uniformity between produ.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)
(discontinued **) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Specific Heat Capacity | 0.900 - 1.10 J/g-°C @Temperature 23.0 °C |
0.215 - 0.263 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Specific Heat Capacity | 0.900 J/g-°C @Temperature 20.0 - 100 °C |
0.215 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
CeramTec Rubalit® A 1896 brown Alumina CeramTec AG's seal and regulator discs are made mainly of Rubalit® A 1896, a material developed especially for this application that is noted for the following special properties: outstanding hard.. |