Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.880 J/g-°C | 0.210 BTU/lb-°F | |
Sapco 95% Aluminum Oxide Information provided by Sapco. |
|||
Specific Heat Capacity | 0.880 J/g-°C | 0.210 BTU/lb-°F | ASTM E1269 |
CoorsTek AD-94 Alumina (nom. 94% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.880 J/g-°C | 0.210 BTU/lb-°F | ASTM E1269 |
CoorsTek AD-96 Alumina (nom. 96% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.880 J/g-°C | 0.210 BTU/lb-°F | ASTM E1269 |
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.880 J/g-°C | 0.210 BTU/lb-°F | ASTM E1269 |
CoorsTek AD-998 Alumina(nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.880 J/g-°C | 0.210 BTU/lb-°F | ASTM E1269 |
CoorsTek FG-995 Alumina (nom. 98.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.880 J/g-°C | 0.210 BTU/lb-°F | ASTM E1269 |
CoorsTek PlasmaPure™ Alumina (nom. 99.8% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |