Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.879 J/g-°C | 0.210 BTU/lb-°F | |
Alcoa QC-10® Aluminum Mold Alloy Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-.. |
|||
Specific Heat Capacity | 0.879 J/g-°C | 0.210 BTU/lb-°F | |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Specific Heat Capacity | 0.879 J/g-°C | 0.210 BTU/lb-°F | |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Specific Heat Capacity | 0.879 J/g-°C | 0.210 BTU/lb-°F | |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |