Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.858 J/g-°C | 0.205 BTU/lb-°F | |
Mateck Glass (BK7 Schott or analogous) Optical crystals |
|||
Specific Heat Capacity | 0.858 J/g-°C | 0.205 BTU/lb-°F | |
Schott N-BK7 Glass Information Provided by SCHOTT North America, Inc. |