Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Osprey Metals CE11 Al-Si Controlled Expansion Alloy
Al-50%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Momentive Performance Materials PolarTherm® PT110 Boron Nitride (BN) Powder
Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarThermâ„¢'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp..
Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Momentive Performance Materials PolarTherm® PT120 Boron Nitride (BN) Powder
Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarThermâ„¢'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp..
Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Momentive Performance Materials PolarTherm® PT140 Boron Nitride (BN) Powder
Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen..
Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Momentive Performance Materials PolarTherm® PT160 Boron Nitride (BN) Powder
Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen..
Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Momentive Performance Materials PolarTherm® PT180 Boron Nitride (BN) Powder
Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic componen..
Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Momentive Performance Materials PolarTherm® PT350 Boron Nitride (BN) Powder
Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon..
Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Momentive Performance Materials PolarTherm® PT370 Boron Nitride (BN) Powder
Low Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic compon..
Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Momentive Performance Materials PolarTherm® PT620 Boron Nitride (BN) Powder
High Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp..
Specific Heat Capacity 0.794 J/g-°C
0.190 BTU/lb-°F
Momentive Performance Materials PolarTherm® PT670 Boron Nitride (BN) Powder
High Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp..
Copyright © lookpolymers.com All Rights Reserved