Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.690 J/g-°C @Temperature 0.000 - 50.0 °C |
0.165 BTU/lb-°F @Temperature 32.0 - 122 °F |
|
Momentive Performance Materials Type 254 Fused Quartz Tubing A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen .. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-BAK2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-BALF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-FK51A Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-KZFS11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-SF6 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | |
Schott N-SF6HT Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.690 J/g-°C | 0.165 BTU/lb-°F | ASTM-E1269 |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |