Polymer Property : Specific Heat Capacity = 0.649 J/g-°C
Polymer Property :
Specific Heat Capacity =
0.649 J/g-°C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Specific Heat Capacity
0.649
J/g-°C
0.155
BTU/lb-°F
Schott N-LAK9 Glass
Information Provided by SCHOTT North America, Inc.