Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.589 J/g-°C @Temperature 800 °C |
0.141 BTU/lb-°F @Temperature 1470 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.589 J/g-°C @Temperature 800 °C |
0.141 BTU/lb-°F @Temperature 1470 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.589 J/g-°C @Temperature 800 °C |
0.141 BTU/lb-°F @Temperature 1470 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.589 J/g-°C @Temperature 800 °C |
0.141 BTU/lb-°F @Temperature 1470 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.589 J/g-°C @Temperature 800 °C |
0.141 BTU/lb-°F @Temperature 1470 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.589 J/g-°C @Temperature 800 °C |
0.141 BTU/lb-°F @Temperature 1470 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.589 J/g-°C @Temperature 800 °C |
0.141 BTU/lb-°F @Temperature 1470 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.589 J/g-°C @Temperature 800 °C |
0.141 BTU/lb-°F @Temperature 1470 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Specific Heat Capacity | 0.589 J/g-°C @Temperature 800 °C |
0.141 BTU/lb-°F @Temperature 1470 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |