Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.506 J/g-°C | 0.121 BTU/lb-°F | |
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Specific Heat Capacity | 0.506 J/g-°C | 0.121 BTU/lb-°F | |
Dura-Bar 80-55-06 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Specific Heat Capacity | 0.506 J/g-°C | 0.121 BTU/lb-°F | |
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i.. |