Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.418 J/g-°C @Temperature 100 °C |
0.100 BTU/lb-°F @Temperature 212 °F |
|
Schmolz + Bickenbach MoldMAX HH® High Hard - Copper Alloy Description: Brush Wellman’s MoldMAX HH® (High Hard) is the premier copper mold alloy. This alloy has a hardness and strength comparable with standard tool steels but its thermal conductivit.. |
|||
Specific Heat Capacity | 0.418 J/g-°C @Temperature 100 °C |
0.100 BTU/lb-°F @Temperature 212 °F |
|
Schmolz + Bickenbach MoldMAX LH® Low Hard - Copper Alloy Description: Brush Wellman’s MoldMAX LH® (Low Hard) is a premium copper mold alloy that provides hardness and strength comparable with standard AISI P-20 tool steel and a thermal conductivit.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.100 BTU/lb-°F | |
Weartech International WT-40 Nickel Hardfacing & Wear Resistant Alloy Applications: glass industry plungers and mold componentsInformation provided by Weartech International |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.100 BTU/lb-°F | |
Weartech International WT-60 Nickel Hardfacing & Wear Resistant Alloy Applications: pump sleevesInformation provided by Weartech International |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.100 BTU/lb-°F | |
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.100 BTU/lb-°F | |
Bohler-Uddeholm BÖHLER S590 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.100 BTU/lb-°F | hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh.. |
|||
Specific Heat Capacity | 0.418 J/g-°C @Temperature 20.0 °C |
0.100 BTU/lb-°F @Temperature 68.0 °F |
|
Carlson 2205 (UNS S31803) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Specific Heat Capacity | 0.418 J/g-°C @Temperature 20.0 °C |
0.100 BTU/lb-°F @Temperature 68.0 °F |
|
Carlson 2205 (UNS S32205) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C (1350°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 732°C/8hr/FC to 621°C/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.100 BTU/lb-°F | |
Carpenter Micro-Melt® HS-30 Alloy Micro-Melt® HS-30 alloy is an 8% cobalt, high hardenability tungsten-molybdenum alloyed high-speed steel exhibiting excellent hot hardness combined with good wear resistance and toughness. The adva.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/4hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Aged 732°C (1350°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Cold Drawn 37.5% Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Cold Drawn 37.5% Plus Aging 649°C (1200°F)/4hr/FC to 579°C/4hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 718°C (1325°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |
|||
Specific Heat Capacity | 0.418 J/g-°C @Temperature 20.0 °C |
0.100 BTU/lb-°F @Temperature 68.0 °F |
|
Assab Steels ASP 23 Cold Work Steel ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope.. |
|||
Specific Heat Capacity | 0.418 J/g-°C | 0.0999 BTU/lb-°F | |
Carpenter Custom Age 625 PLUS® Nickel-Base Alloy, Double Aged 746°C (1375°F)/8hr/AC to 621°C (1150°F)/8hr/AC Data provided by Carpenter Technology Corporation.Custom Age 625 PLUS® alloy is a precipitation hardenable, nickel-base alloy which, in many environments, displays corrosion resistance similar to t.. |