Polymer Property : Specific Heat Capacity = 0.409 J/g-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.409 J/g-°C

@Temperature 200 °C
0.0978 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.409 J/g-°C

@Temperature 200 °C
0.0978 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.409 J/g-°C

@Temperature 200 °C
0.0978 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.409 J/g-°C

@Temperature 200 °C
0.0978 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.409 J/g-°C

@Temperature 200 °C
0.0978 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.409 J/g-°C

@Temperature 200 °C
0.0978 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.409 J/g-°C

@Temperature 200 °C
0.0978 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.409 J/g-°C

@Temperature 200 °C
0.0978 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, 6.3 mm plate
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Specific Heat Capacity 0.409 J/g-°C

@Temperature 200 °C
0.0978 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..