Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.150 J/g-°C | 0.0359 BTU/lb-°F | Solid |
Indium Corp. Indalloy® 182 Au-Sn Solder Alloy Eutectic die attach and package sealing.Information provided by the manufacturer, Indium Corporation. |
|||
Specific Heat Capacity | 0.150 J/g-°C | 0.0359 BTU/lb-°F | Solid |
Indium Corp. Indalloy® 233 Pb-Sb-Sn Solder Alloy Intermediate temp solder. Creep resistant.Information provided by the manufacturer, Indium Corporation. |