Polymer Property : Annealing Point = 981 °F
Polymer Property :
Annealing Point =
981 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Annealing Point
527
°C
981
°F
Schott S8801 Contrast Enhancement Filter
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.