Thermal Properties Metric English Comments
Annealing Point 490 °C
914 °F
Ferro EG 3600 Metal Sealing
Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Compress.Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se..
Annealing Point 490 °C
914 °F
Ferro F 2719 Metal Sealing
Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Kovar Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals..
Annealing Point 490 °C
914 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Schott Glass 8652 Sealing Glass
Tungsten sealing glass, lower sealing temperature than glass 8651 Power diodesInformation provided by SCHOTT AG.
Annealing Point 490 °C
914 °F
Ferro EG 2964 Glaze and Sealant Glass
Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ins..