Polymer Property : Annealing Point = 176 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Annealing Point 80.0 - 90.0 °C
176 - 194 °F
3-5 hours
LG Chemical EG920 PMMA, General Purpose Grade for Extrusion
General purpose grade with excellent stress cracking resistanceIntended mainly for exterior applicationsRecommended mainly for sheets, pipes, and profilesFeatures: Excellent transparency and eleganc..
Annealing Point 80.0 - 90.0 °C
176 - 194 °F
3-5 hours
LG Chemical EH910 PMMA, General Purpose Grade for Extrusion
Excellent solvent resistanceHighest of all grades in heat resistance, mechanical strength, surface hardness and stress cracking resistanceFeatures: Excellent transparency and eleganceWeather resista..
Annealing Point 80.0 - 90.0 °C
176 - 194 °F
3-5 hours
LG Chemical IH830A PMMA, General Purpose Grade for Injection Molding
Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and ..
Annealing Point 80.0 - 90.0 °C
176 - 194 °F
3-5 hours
LG Chemical IH830C PMMA, General Purpose Grade for Injection Molding
Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and ..
Annealing Point 80.0 - 90.0 °C
176 - 194 °F
3-5 hours
LG Chemical IH830H PMMA, General Purpose Grade for Injection Molding
Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and ..
Annealing Point 80.0 - 90.0 °C
176 - 194 °F
3-5 hours
LG Chemical IH830 PMMA, General Purpose Grade for Injection Molding
Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and ..