Polymer Property : Annealing Point = 60.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Annealing Point 60.0 - 90.0 °C
140 - 194 °F
Average value: 77.1 °C Grade Count:7
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Annealing Point 60.0 - 70.0 °C
140 - 158 °F
3-5 hours
LG Chemical HI835HS PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Annealing Point 60.0 - 70.0 °C
140 - 158 °F
3-5 hours
LG Chemical HI835S PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Annealing Point 60.0 - 70.0 °C
140 - 158 °F
3-5 hours
LG Chemical HI855H PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Annealing Point 60.0 - 70.0 °C
140 - 158 °F
3-5 hours
LG Chemical HI855HS PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Annealing Point 60.0 - 70.0 °C
140 - 158 °F
3-5 hours
LG Chemical HI855M PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Annealing Point 60.0 - 70.0 °C
140 - 158 °F
3-5 hours
LG Chemical HI855S PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Annealing Point 60.0 - 70.0 °C
140 - 158 °F
3-5 hours
LG Chemical IF850 PMMA, General Purpose Grade for Injection Molding
High flowability gradeParticularly recommended for complicated profiles or large and thin wall partsFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface har..
Annealing Point 60.0 °C
140 °F
3-5 hours
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding
Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha..
Annealing Point 60.0 - 70.0 °C
140 - 158 °F
Average value: 65.0 °C Grade Count:8
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Annealing Point 60.0 - 70.0 °C
140 - 158 °F
3-5 hours
LG Chemical HI835H PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Annealing Point 60.0 - 70.0 °C
140 - 158 °F
3-5 hours
LG Chemical HI835M PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Copyright © lookpolymers.com All Rights Reserved