Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | >= 260 °C | >= 500 °F | ASTM Test |
Lubriplate 1552 Lithium Complex Multi-Purpose Grease These multi-purpose lithium complex lubricants can withstand higher temperatures than traditional lithium greases. They provide high film strength, excellent shear stability, long lubricant life, an.. |
|||
Dropping Point | 260 °C | 500 °F | ASTM Test |
Lubriplate HP-2 Poly Polyurea-Thickened Type Grease For Special Applications / Conditions Polyurea-thickened type grease formulated with the highest quality paraffinic base oils available. Excellent for high speed electric motor bearings and other industrial applications. Applications: E.. |
|||
Dropping Point | 260 °C | 500 °F | ASTM Test |
Lubriplate SYN SYN-1600 PAO-Based Multi-Purpose Grease Manufactured with 100% PAO base fluids and thickened with lithium complex for superior oxidation stability, better wear protection, and significantly better operating temperature ranges. Fortified w.. |
|||
Dropping Point | 260 °C | 500 °F | ASTM Test |
Lubriplate SYN SYN-1601 PAO-Based Multi-Purpose Grease Manufactured with 100% PAO base fluids and thickened with lithium complex for superior oxidation stability, better wear protection, and significantly better operating temperature ranges. Fortified w.. |
|||
Dropping Point | >= 260 °C | >= 500 °F | ASTM D2265 |
ExxonMobil 100 Mobiltemp SHC Series Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base .. |
|||
Dropping Point | >= 260 °C | >= 500 °F | ASTM D2265 |
ExxonMobil 100 Special Mobiltemp SHC Series Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base .. |
|||
Dropping Point | 260 °C | 500 °F | ASTM D2265 |
ExxonMobil CM-P Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Dropping Point | 260 °C | 500 °F | ASTM D2265 |
ExxonMobil Mobil Polyrex EM Super-premium Mobil Polyrex EM Series grease is specially formulated for electric-motor bearings. The advanced thickener formulation and proprietary manufacturing techniques provide improved bearing.. |
|||
Dropping Point | >= 260 °C | >= 500 °F | |
ConocoPhillips Syncon® Extra Long Life Grease NLGI No. 00 Description: Conoco Syncon Extra Long Life Grease is an ultra high performance lithium-complex grease with heavy synthetic base oil specifically designed for long service life under heavily loaded c.. |
|||
Dropping Point | 260 °C | 500 °F | |
ConocoPhillips Tacna® HD Grease NLGI Grade 1 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Dropping Point | >= 260 °C | >= 500 °F | |
ConocoPhillips Tacna® HD Grease NLGI Grade 2 Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recomm.. |
|||
Dropping Point | 260 °C | 500 °F | ASTM D-2265 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 0 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Dropping Point | >= 260 °C | >= 500 °F | |
Dow Corning MOLYKOTE® AS-880N GREASE Silicone grease especially for brake pad shimInformation provided by Dow Corning |
|||
Dropping Point | 260 °C | 500 °F | ASTM D2265 |
Chesterton 629 High Temperature White Grease Description: Superior resistance to washout by water, caustics, sanitizing cleaners, process fluids and steam has now been combined with high temperature performance to produce Chesterton 629 High T.. |
|||
Dropping Point | >= 260 °C | >= 500 °F | |
Dow Corning MOLYKOTE® G-0101 Rolling element bearing grease for high speed applicationInformation provided by Dow Corning |
|||
Dropping Point | 260 °C | 500 °F | |
ChevronTexaco RPM® NLGI 1 Heavy Duty LC Grease EP FeaturesChevron RPM Heavy Duty LC Greases EP are multipurpose, water resistant, extreme pressure, heavy duty chassis, wheel bearing, and general purpose lubricating greases.They are manufactured usi.. |
|||
Dropping Point | 260 °C | 500 °F | |
ChevronTexaco Starplex® Moly NLGI Grade 1 Texaco Starplex Moly greases deliver value through:Good water resistance — Seals out water, reducing rust and corrosion.Extreme pressure protection.Protection against shock loading — extending veh.. |
|||
Dropping Point | >= 260 °C | >= 500 °F | |
ChevronTexaco Thermatex® EP NLGI Grade 1 Texaco Thermatex EP greases deliver value through:High temperature stability — Will not melt at high temperatures, but will remain in place on bearing surfaces and continue to provide excellent lub.. |
|||
Dropping Point | 260 °C | 500 °F | ASTM D2265 |
ExxonMobil 221 Mobilgrease FM Mobilgrease FM 221 and FM 222 are high performance multi-purpose products designed specifically for the lubrication of food processing machinery. Mobilgrease FM 221 and FM 222 are formulated with co.. |
|||
Dropping Point | 260 °C | 500 °F | ASTM D2265 |
ExxonMobil 3 Mobilith AW Series The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Dropping Point | >= 260 °C | >= 500 °F | ASTM D2265 |
ExxonMobil 32 Mobiltemp SHC Series Mobiltemp SHC Series products are supreme performance antiwear greases primarily intended for high temperature applications. They combine the unique features of polyalphaolefin (PAO) synthetic base .. |
|||
Dropping Point | 260 °C | 500 °F | ASTM D2265 |
ExxonMobil CM-W Mobilgrease CM Series Mobilgrease CM Series products are a family of high performance extreme-pressure greases. Mobilgrease CM-P and CM-S are NLGI Grade 2, while Mobilgrease CM-W and CM-L are NLGI Grade 1. All four produ.. |
|||
Dropping Point | 260 °C | 500 °F | ASTM D2265 |
ExxonMobil Mobil Polyrex EM Super-premium Mobil Polyrex EM Series grease is specially formulated for electric-motor bearings. The advanced thickener formulation and proprietary manufacturing techniques provide improved bearing.. |
|||
Dropping Point | >= 260 °C | >= 500 °F | |
ConocoPhillips 2 Super Lube M EP Grease NLGI No. Description: Conoco Super Lube M EP Grease is a premium-quality, multipurpose, high-temperature, extreme-pressure (EP) lithium complex grease developed to satisfy the severe requirements of off-road.. |
|||
Dropping Point | 260 °C | 500 °F | |
ConocoPhillips EP Conolith® HT Grease NLGI NO.2 Description: Conoco EP Conolith HT Grease is a premium-quality, lithium-complex, multipurpose, extreme-pressure, high-temperature grease developed to satisfy the severe requirements of high-speed wh.. |
|||
Dropping Point | 260 °C | 500 °F | ASTM D2265 |
ExxonMobil 2 Mobilith AW Series The Mobilith AW Series products are high performance lithium-complex greases. They are formulated with antiwear agents to provide excellent service under the severe operating conditions of heavy and.. |
|||
Dropping Point | 260 °C | 500 °F | |
ConocoPhillips EP Polyurea NLGI Grade No. 2 Polyurea Greases offer significant performance advantages in high temperature, multipurpose, long-life and wet applications over conventional soap thickened greases. The nonsoap, polyurea thickener,.. |
|||
Dropping Point | 260 °C | 500 °F | ASTM D-2265 |
ConocoPhillips Tacna® M5 Grease NLGI Grade 2 Description: Conoco Tacna M5 Grease is a high-performance, lithium-complex grease with 5% molybdenum disulfide specifically designed for extreme loading conditions. The combination of highly refined.. |
|||
Dropping Point | 260 °C | 500 °F | |
ConocoPhillips Tacna® Rx NLGI No. 2 Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor.. |
|||
Dropping Point | 260 °C | 500 °F | |
ChevronTexaco Rykon® NLGI 1 Premium Grease EP FeaturesChevron Rykon Premium Grease EP is a high quality, water resistant, extreme pressure, multipurpose lubricating grease.It is manufactured using highly refined, select high viscosity index bas.. |