Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 199 °C | 390 °F | ASTM Test |
Lubriplate 630-A Lithium Based Multi-Purpose Grease These popular lithium type greases are excellent for a wide range of lubrication demands thus reducing the need to carry large grease inventories. They show exceptional resistance to water, steam, a.. |
|||
Dropping Point | 199 °C | 390 °F | ASTM Test |
Lubriplate EMB Lithium-Polymer Type Grease For Special Applications / Conditions Lithium polymer type grease developed specifically for the lubrication of electric motor bearings, fans, and other high speed grease type ball and roller bearings. Applications: Electric motor beari.. |
|||
Dropping Point | 199 °C | 390 °F | ASTM D566 |
Chesterton 613 Moly Grease Description: Chesterton® 613 Moly Grease is a high-performance, cost-effective lubricant that can withstand extreme temperatures and pressures for a wide range of high and low-speed applications. F.. |
|||
Dropping Point | 199 °C | 390 °F | |
ELM® TempFlex™ 35 to 160 Biodegradable Rail Curve Lubricant Description: TempFlex™ 35 to 160 is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA-grown vegetable oils and a lithiumbased thickener.Applications: Designed.. |
|||
Dropping Point | 199 °C | 390 °F | |
ELM® TempFlex™ 35 to 160 w/ MoS2 Biodegradable Rail Curve Lubricant Description: TempFlex™ 35 to 160 now with molybdenum disulphide is a premium quality biodegradable, Biotechbased™ Rail Curve Lubricant formulated from USA grown vegetable oils and a lithium-based .. |