Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 52.0 - 60.0 °C | 126 - 140 °F | |
Struktol V-PEAS LA LUBRICANT ADDITIVE FOR PVC AND POLYMER PROCESSING STRUKTOL® V-PEAS LA is a very effective lubricant with externally lubricating properties which has no negative impact on clarity in extrusion, calendering, or injection molding. STRUKTOL® V-PE.. |
|||
Dropping Point | 52.0 - 60.0 °C | 126 - 140 °F | |
Struktol V-PEAS Processing Additive Polymeric complex ester of saturated fatty acids.Typical Applications: STRUKTOL® V-PEAS is a very compatible complex ester lubricant. It has noted performance in clear–calendared sheet. It a.. |
|||
Dropping Point | 52.0 - 60.0 °C | 126 - 140 °F | |
Struktol V-PEAS VG LUBRICANT ADDITIVE FOR PVC AND POLYMER PROCESSING STRUKTOL® V-PEAS VG is a very effective lubricant with externally lubricating properties which has no negative impact on clarity in extrusion, calendaring, or injection molding. STRUKTOL® V-PE.. |