Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 300 °C | 572 °F | ASTM D2265 |
ExxonMobil 1 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Dropping Point | 300 °C | 572 °F | ASTM D2265 |
ExxonMobil 2 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Dropping Point | 300 °C | 572 °F | ASTM D2265 |
ExxonMobil 78 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Dropping Point | >= 300 °C | >= 572 °F | ASTM D2265 |
ExxonMobil Mobil Infinitec 152 Mobil Infinitec 152 super-long-life grease, recommended for a wide range of automotive and industrial applications, represents a major advance in lithium-complex grease technology. Developed and pat.. |
|||
Dropping Point | >= 300 °C | >= 572 °F | |
Dow Corning MOLYKOTE® 3452 CHEMICAL RESISTANT VALVE GREASE Fluorosilicone grease thickened with PTFEInformation provided by Dow Corning |
|||
Dropping Point | >= 300 °C | >= 572 °F | |
Dow Corning MOLYKOTE® 41 HIGH TEMPERATURE BEARING GREASE Phenyl-methyl silicone grease thickened with carbon blackInformation provided by Dow Corning |
|||
Dropping Point | 300 °C | 572 °F | ASTM D2265, DIN 51 801/1 |
Chesterton 615 HTG #1 Grease Description: Chesterton® 615 HTG #1 is the versatile performer needed in all applications requiring a heavy duty NLGI #1 grease. The outstanding extreme pressure characteristic of this grease, cou.. |
|||
Dropping Point | >= 300 °C | >= 572 °F | |
Dow Corning MOLYKOTE® G-0102 Heavy duty bearing grease for applications in presence of waterInformation provided by Dow Corning |
|||
Dropping Point | 300 °C | 572 °F | ASTM D2265 |
ExxonMobil 1 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Dropping Point | 300 °C | 572 °F | ASTM D2265 |
ExxonMobil 2 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Dropping Point | 300 °C | 572 °F | ASTM D2265 |
ExxonMobil 78 Mobiltemp Series Mobiltemp Series greases are high performance clay-thickened products designed for the lubrication of plain and antifriction bearings operating at low speed and high temperature or under cycling con.. |
|||
Dropping Point | >= 300 °C | >= 572 °F | ASTM D2265 |
ExxonMobil Mobil Infinitec 152 Mobil Infinitec 152 super-long-life grease, recommended for a wide range of automotive and industrial applications, represents a major advance in lithium-complex grease technology. Developed and pat.. |
|||
Dropping Point | 300 °C | 572 °F | |
Dow Corning 340 Heat Sink Compound White, non-flowing, highly filled compound, good thermal conductivity.Information provided by Dow Corning |