Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 232 °C | 450 °F | ASTM Test |
Lubriplate 1550 Lithium Complex Multi-Purpose Grease These multi-purpose lithium complex lubricants can withstand higher temperatures than traditional lithium greases. They provide high film strength, excellent shear stability, long lubricant life, an.. |
|||
Dropping Point | 232 °C | 450 °F | ASTM Test |
Lubriplate 3000 Moly-Lithium Type Multi-Purpose Grease Tacky, moly-lithium, extreme pressure greases that provide a durable, tenacious, adhesive film to protect against water, rust, and corrosive contaminants. 3000-W is for cold ambient temperatures.App.. |
|||
Dropping Point | 232 °C | 450 °F | ASTM Test |
Lubriplate CLEARPLEX 2 Aluminum Complex USP Mineral Oil-Based Food Machinery Grade Grease This Aluminum Complex thickened, H-1 class grease is engineered for use in plain and anti-friction bearings in the food-processing and beverage processing industry. Contains non zinc-oxide anti-wear.. |
|||
Dropping Point | 232 °C | 450 °F | ASTM Test |
Lubriplate FGL CC Aluminum Complex USP Mineral Oil-Based Food Machinery Grade Grease High performance, multi-purpose food grade grease designed to meet the demands of food and beverage industry plant engineers who want Class H-1 greases to totally replace H-2 greases. Fortified with.. |
|||
Dropping Point | 232 °C | 450 °F | ASTM Test |
Lubriplate SFL-1 Aluminum Complex Synthetic Food Machinery Grade Grease This series provides an exceptionally wide operating temperature range, high shear stability, excellent water resistance, and load carrying properties. For use in freezers and other cold temperature.. |
|||
Dropping Point | 232 °C | 450 °F | |
ChevronTexaco Starplex® HD 6802 NLGI Grade 2 Texaco Starplex HD 6802 delivers value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protecti.. |
|||
Dropping Point | 232 °C | 450 °F | |
ChevronTexaco Texclad® 2 Texaco Texclad 2 delivers value through:Water tolerance — Resists washout, even when subject to gross water contamination.Excellent adhesiveness — Assures good film strength even in a wet environm.. |
|||
Dropping Point | 232 °C | 450 °F | |
ChevronTexaco Thread Sealing Compound FeaturesChevron Thread Sealing Compound is a time-tested aluminum complex grease designed especially for casing and tubing connections in high-pressure oil well service, or wherever unusually severe.. |
|||
Dropping Point | 232 °C | 450 °F | |
ChevronTexaco Tool Joint Compound FeaturesChevron Tool Joint Compound is an aluminum complex grease designed principally for the lubrication of drill collars, tool joints and pipe threads.It contains copper flake and graphite, forti.. |
|||
Dropping Point | 232 °C | 450 °F | |
ConocoPhillips 1 Milube® Grease 2100 NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |
|||
Dropping Point | 232 °C | 450 °F | ASTM D-566 |
ConocoPhillips ANDEROL® 40 AA-2 Grease, White Mineral Food Grade NLGI 2 Description: ANDEROL PQ 40 AA Greases are aluminum complex thickened, white mineral oil-based products that meet the former H-1 approval requirements of the USDA where incidental food contact can oc.. |
|||
Dropping Point | 232 °C | 450 °F | ASTM D-566 |
ConocoPhillips ANDEROL® 783-1 Series Synthetic Food Grade Greases, NLGI Grade 1 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Dropping Point | 232 °C | 450 °F | |
ChevronTexaco Starplex® Premium NLGI Grade 1 Texaco Starplex Premium delivers value through:Continuous high temperature stability up to 325°F.Excellent corrosion and wear protection.Excellent water resistance.Extended relubrication intervals .. |
|||
Dropping Point | 232 °C | 450 °F | |
ConocoPhillips 1 Milube® Grease 2100T NLGI No. 1 Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic .. |