Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 230 °C | 446 °F | ASTM D2265 |
ExxonMobil Unirex N 2 UNIREX N greases are premium-quality, lithium-complex products suitable for high-temperature service in rolling-element bearings. These versatile greases can be used in a wide range of industrial ap.. |
|||
Dropping Point | 230 °C | 446 °F | ASTM D2265 |
ExxonMobil Unirex N 3 UNIREX N greases are premium-quality, lithium-complex products suitable for high-temperature service in rolling-element bearings. These versatile greases can be used in a wide range of industrial ap.. |
|||
Dropping Point | 230 °C | 446 °F | |
Dow Corning MOLYKOTE® AS-810 GREASE Silicone grease with wide service temperature range for starter clutchInformation provided by Dow Corning |
|||
Dropping Point | 230 °C | 446 °F | ASTM D2265 |
ExxonMobil Unirex N 2 UNIREX N greases are premium-quality, lithium-complex products suitable for high-temperature service in rolling-element bearings. These versatile greases can be used in a wide range of industrial ap.. |
|||
Dropping Point | 230 °C | 446 °F | ASTM D2265 |
ExxonMobil Unirex N 3 UNIREX N greases are premium-quality, lithium-complex products suitable for high-temperature service in rolling-element bearings. These versatile greases can be used in a wide range of industrial ap.. |
|||
Dropping Point | 230 °C | 446 °F | |
ChevronTexaco Delo® Synthetic Grease SF FeaturesChevron Delo Synthetic Grease SF is a high performance grease specifically engineered for trailer wheel-ends operating in all conditions, even under the most extreme high and low temperature.. |