Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 170 °C | 338 °F | ASTM D2265 |
ExxonMobil Greasrex K-192 Greasrex K-192 is a high performance extreme pressure lithium hydroxystearate grease, which provides excellent protection against rust, corrosion and wear. It is formulated especially for use in a.. |
|||
Dropping Point | 170 °C | 338 °F | |
ELM® White Lithium Biodegradable Lubricating Grease Description: White Lithium Grease is premium quality biodegradable, Biotechbased™ multipurpose grease formulated from USA-grown vegetable oils and a lithiumbased thickener.Applications: Designed f.. |
|||
Dropping Point | 170 °C | 338 °F | ASTM D2265 |
ExxonMobil Greasrex K-192 Greasrex K-192 is a high performance extreme pressure lithium hydroxystearate grease, which provides excellent protection against rust, corrosion and wear. It is formulated especially for use in a.. |